Polycrystalline samples of NaxCo2O4 were synthesized by conversional solidstate reaction (SSR) method, various temperatures sintered at of 1173- 1293 K. The mechanical properties of the samples showed the crystal structure, elastic moduli and Debye temperature. The thermoelectric properties of the samples obtained the electrical resistivity, Seebeck coefficient and thermal conductivity are increases with increased sintering temperature. The dimensionless figure of merit was decreased with an increase in sintering temperature, and the sample sintered at 1173 K was a maximum values, ZT ∼ 0.11 at 973 K.


Isenção de responsabilidade: Este resumo foi traduzido usando ferramentas de inteligência artificial e ainda não foi revisado ou verificado

Indexado em

  • CASS
  • Google Scholar
  • Abra o portão J
  • Infraestrutura Nacional de Conhecimento da China (CNKI)
  • CiteFactor
  • Cosmos SE
  • Biblioteca de Periódicos Eletrônicos
  • Diretório de indexação de periódicos de pesquisa (DRJI)
  • Laboratórios secretos de mecanismos de pesquisa
  • ICMJE

Veja mais

Flyer