Synthesis and characterization of new polyamides bearing á,á-xylyldithiophenoxide units in the main chain: Microwave irradiation, nanostructures

Esmael Rostami, Abdolkarim Zare, Masume Zangooei


Newpolyamides containing á,áï‚¢-Xylyldithiophenoxide Unitswere prepared under microwave irradiation and their solubility, thermal behavior, viscosities and nanostructures were evaluated. These polyamides showed good solubility in a series of organic solvents. The viscosities of these polyamides are in the range of 0.41-0.54 dl/g. Glass transition temperatures are in the range of 214-251°C. Temperatures for 10% weight loss (T10) are in the range of 286-323°C, temperatures for 50% weight loss (T50) are in the range of 463-535°C and char yields are in the range of 21-41%; and these results shows the thermal stabilities of the prepared polyamides. Supramolecular assemblies showed nanostructures.


Isenção de responsabilidade: Este resumo foi traduzido usando ferramentas de inteligência artificial e ainda não foi revisado ou verificado

Indexado em

  • CASS
  • Google Scholar
  • Abra o portão J
  • Infraestrutura Nacional de Conhecimento da China (CNKI)
  • CiteFactor
  • Cosmos SE
  • Diretório de indexação de periódicos de pesquisa (DRJI)
  • Laboratórios secretos de mecanismos de pesquisa
  • Fator de impacto do artigo acadêmico (SAJI))
  • ICMJE

Veja mais

Flyer